Figure 5From: In vitro corrosion of ZEK100 plates in Hank's Balanced Salt Solution SEM pictures of the cross-section area. a) 2 weeks, b) 4 weeks c) 6 weeks. The corrosion pits are marked by black arrows.Back to article page