Skip to main content

Table 8 Ultimate tensile strength (UTS) of collagen-rich tissues, decellularized, and further processed materials

From: Processing of collagen based biomaterials and the resulting materials properties

Material UTS (MPa) Refs.
Raw material
 Tendon 30–300 [47, 497]
 Ligament 30–300
 Aorta 0.3–1.7
 Skin 1–16
 Pericard 3–18 [498]
Decellularized
 SIS based 3–22 [499, 500]
 Dermis based 10–39 [40, 252, 500, 501]
 Pericard 8–32 [252, 500, 502]
Cast
 Thread 2–56 [265, 503]
 Film 30–40 [250]
 Sponge 0.001 [504]