From: Note on the use of different approaches to determine the pore sizes of tissue engineering scaffolds: what do we measure?
Parameters of the scaffolds cross-linking
Temperature
Genipin/collagen concentration
Abbreviation
20 °C
0.67 g/1 g
RT MAX
0.053 g/1 g
RT MID
0.026 g/1 g
RT MIN
37 °C
37 MAX
37 MID
37 MIN
Non-cross-linked
ORIG