Skip to main content
Figure 4 | BioMedical Engineering OnLine

Figure 4

From: Comparisons of maximum deformation and failure forces at the implant–abutment interface of titanium implants between titanium-alloy and zirconia abutments with two levels of marginal bone loss

Figure 4

SEM of implant surfaces with exposure distances of 3.0 and 1.5 mm. (A) titanium implant in Group A1, (B) titanium implant in Group A2, (C) titanium implant with failed titanium-alloy abutment screw in Group B1, and (D) titanium implant with failed titanium-alloy abutment screw in Group B2. Stars indicate failed abutment screws, and arrows point to the damaged external hexagon of the implant.

Back to article page